SPD Tech Circuit Protection Devices & Solutions
中文

Epoxy Encapsulant

· 5 min
EpoxyPottingEncapsulantTgInsulation

Two-component epoxy potting / encapsulation: curing mechanism, key properties (Tg, CTE, moisture absorption), the link to circuit protection (withstand voltage, moisture, thermal) and typical failures.

Epoxy encapsulant is one of the main materials used for internal device packaging and whole-unit potting in circuit-protection components. It encapsulates a device (SPD, relay, module) or an entire PCB in an insulating resin, providing mechanical protection + electrical isolation + moisture barrier + thermal path in one.

Material system & curing

Type Notes Typical use
Two-part liquid epoxy (A+B) RT or heated cure, higher CTE, moderate cost Potting / local encapsulation
Two-part thermal epoxy Filled with Al₂O₃ / AlN, 0.8–2 W/mK Power modules, IGBT potting
One-part epoxy (moisture-cure) Short pot life, more brittle Spot dispensing, local sealing

After cure, glass-transition temperature (Tg) sets the upper working limit; CTE mismatch with the metal / silicon inside creates thermomechanical stress, the root cause of long-term cycling cracks.

Key properties

  • Tg: 120–180 °C (standard) / 180–220 °C (modified). Pick Tg ≥ 20 °C above the device's peak junction temperature.
  • Volume resistivity: 10¹³ Ω·cm order — the basis for withstand voltage and moisture resistance.
  • CTE: 50–80 ppm/°C, one order of magnitude above copper (17) and silicon (2.6); long-term thermal cycling causes delamination / cracking at the interface.
  • Moisture uptake: < 0.1% (volume), better than silicone; insulation holds up better in cold + high-humidity environments.
  • Thermal conductivity: pure epoxy ~0.2 W/mK; filled types reach 1–2 W/mK — mandatory for power-device potting.
  • Flame retardancy: UL 94 V-0 requires a halogen-free FR formulation.
  • Epoxy potting inside MOV / GDT / TVS mainly provides mechanical fixation + insulation + moisture barrier.
  • If the epoxy Tg is below the device's peak junction temperature, CTE-mismatch stress accumulates and the grain interface cracks → leakage-current drift is a typical failure.
  • Overvoltage devices potting must withstand ≥ 1500 V / 1 min power-frequency (IEC 61643-1 isolation); epoxy is more likely to pass than silicone.

Selection notes

  1. Tg limit: pick the device junction temperature + 20 °C margin.
  2. CTE match: when the CTE of the body (copper post, Al base) is known, choose a lower-CTE modified epoxy, gradient filler where needed.
  3. Moisture / humidity: outdoor / high-humidity — prefer two-part liquid epoxy, avoid one-part moisture-cure.
  4. Flame retardancy: UL 94 V-0 minimum; halogen-free is greener.
  5. Process window: two-part potting mix ratio 1:1 to 3:1, working time 30–60 min after mixing — follow the vendor datasheet.

Common failures

Epoxy potting thermal-cycling cracks (CTE mismatch at the interface), surface leakage after moisture uptake (cold + high humidity + contamination), and incomplete cure (too-low working temperature / wrong mix ratio) are the top three — design them out at material selection.